How PLLA Spherulites Fragment or Disintegrate Under Deformation: Insights from AFM

What happens to the crystalline structures inside a semicrystalline polymer when the material is stretched? A study by Xabier Larrañaga and colleagues, published in Macromolecules, reveals two contrasting deformation pathways in poly(L-lactic acid) (PLLA): fragmentation, in which crystalline order is locally retained, and mechanical disintegration, in which the structure becomes substantially less ordered. Atomic force microscopy (AFM), combined with Raman spectroscopy and polarized-light microscopy, helps explain these different responses.

Physical aging and the deformation of PLLA

PLLA is a polymer whose mechanical response depends strongly on its molecular structure and processing history. In semicrystalline PLLA, ordered structures called spherulites coexist with less ordered, amorphous regions. How these components interact under mechanical stress influences whether the material fractures or undergoes plastic deformation.

An important factor is physical aging. As the amorphous polymer relaxes toward a lower-energy state over time, molecular mobility can become more restricted, making plastic deformation more difficult under the investigated conditions.

Larrañaga and colleagues examined two related aspects of PLLA deformation: the influence of controlled physical aging on the brittle-to-ductile transition of glassy PLLA, and the deformation behaviour of spherulites in semicrystalline PLLA. These were distinct experimental investigations.

In the glassy PLLA experiments, the least-aged samples exhibited a brittle-to-ductile transition at −30 °C, whereas more strongly aged samples required higher temperatures to deform in a ductile manner under the reported testing conditions.

These findings provide context for understanding the importance of the amorphous chain network in polymer deformation, while the separate semicrystalline experiments reveal how spherulites respond when the surrounding material undergoes plastic deformation.

Two deformation pathways: fragmentation and disintegration

When semicrystalline PLLA films were stretched, the researchers observed two distinct responses of the spherulites.

In fragmentation, a spherulite separates into smaller regions, while characteristic crystalline structure remains locally preserved within the fragments.

In mechanical disintegration, the response is different. The former spherulite remains recognizable, but its crystalline structure undergoes substantial disordering during deformation.

The authors interpret these contrasting pathways in terms of the mechanical interaction between crystalline regions and the surrounding amorphous chain network. They propose that connectivity through bridging polymer chains plays a role in whether crystalline domains separate into fragments or undergo more extensive structural rearrangement.

To examine these changes at a local scale, the researchers combined AFM surface imaging with mechanical measurements.

Tapping-mode AFM provided information about surface topography, while AFM force–displacement measurements and nanoindentation-derived Young’s modulus maps revealed variations in local stiffness.

Young’s modulus describes a material’s resistance to elastic deformation. Mapping this property across a deformed spherulite helps distinguish mechanically different regions that may not be apparent from surface morphology alone.

In fragmented spherulites, the AFM measurements revealed alternating regions of higher and lower stiffness. Locally stiff domains reached approximately 2.4 GPa. Together with the complementary Raman evidence, these measurements support the interpretation that crystalline regions remained within the fragments.

The mechanically disintegrated spherulites showed a different response.

Although the former spherulite could still be identified in the AFM topography, its measured stiffness was much closer to that of the surrounding amorphous material. The reported AFM-derived Young’s modulus was 1.01 ± 0.35 GPa for the disintegrated spherulite, compared with 0.92 ± 0.14 GPa for adjacent amorphous regions.

This reduced mechanical contrast is consistent with substantial structural reorganization. It does not mean that the spherulite had physically disappeared or that the two regions were mechanically identical.

Two stacked AFM maps of a disintegrated PLLA spherulite: grayscale surface topography above and orange Young’s modulus map below, with measurement scales.
AFM topography (upper map) and nanoindentation-derived Young’s modulus (lower map) of a mechanically disintegrated PLLA spherulite. Figure 5b excerpt reproduced from Larrañaga et al., Macromolecules (2026), DOI: 10.1021/acs.macromol.6c00777, CC BY 4.0. Panel extracted from the original figure; scientific content unchanged.

AFM probes used in the study

For AFM imaging and force–displacement measurements, the authors used noncoated silicon NanoWorld Pointprobe® NCH AFM probes.

The study combined tapping-mode topography with local force measurements to examine the relationship between surface morphology and nanomechanical response in deformed PLLA.

Raman spectroscopy provides complementary structural evidence

While AFM revealed changes in morphology and local stiffness, these measurements alone could not establish whether crystalline order had been retained or lost.

The researchers therefore used polarized Raman spectroscopy to investigate changes in molecular structure.

For fragmented spherulites, Raman spectra retained characteristic signatures of crystalline PLLA within the separated regions. This supported the interpretation that fragmentation had occurred without complete loss of local crystalline organization.

In mechanically disintegrated spherulites, several characteristic crystalline Raman features disappeared or became substantially weaker. The spectra instead showed features more consistent with a deformed, less ordered molecular structure. This indicates substantial disordering rather than necessarily proving the complete disappearance of all crystalline material.

Together, the AFM and Raman results distinguish mechanical fragmentation from the more extensive structural disordering associated with spherulite disintegration. Polarized-light microscopy provided additional context for the deformation morphology.

Understanding ductility in semicrystalline polymers

The study highlights why the mechanical behaviour of PLLA cannot be understood from crystallinity alone.

The experiments on glassy PLLA demonstrate the influence of physical aging on the brittle-to-ductile transition under the investigated conditions. The separate semicrystalline experiments show how interactions between crystalline regions and the amorphous chain network are associated with contrasting deformation responses.

By combining local AFM measurements with complementary structural characterization, Larrañaga and colleagues connect changes in morphology and stiffness with their interpretation of the underlying deformation mechanisms.

The findings contribute to a more detailed understanding of how molecular organization, physical aging and interactions between crystalline and amorphous regions influence the mechanical response of PLLA.

Full Citation

Xabier Larrañaga, Brian J. Rodriguez, Jose R. Sarasua and Ester Zuza
Against the Segmental Relaxation of the Chain Network: Activating the Ductile Mechanism of Both Glassy and Semicrystalline PLLA
Macromolecules 2026
https://doi.org/10.1021/acs.macromol.6c00777

Creative Commons Attribution 4.0 International (CC BY 4.0)
https://creativecommons.org/licenses/by/4.0/

Lateral Piezoelectricity of Alzheimer‘s Aβ Aggregates

Alzheimer’s disease (AD) is the most frequent neurodegenerative disorder in the elderly aged over 65.*

The extracellular accumulation of beta-amyloid (Aβ) aggregates in the brain is considered as the major event worsening the AD symptoms, but its underlying reason has remained unclear.

In the article „Lateral Piezoelectricity of Alzheimer‘s Aβ Aggregates“ by Jinhyeong Jang, Soyun Joo, Jiwon Yeom, Yonghan Jo, Jingshu Zhang, Seungbum Hong and Chan Beum Park the piezoelectric characteristics of Aβ aggregates are revealed.

The vector piezoresponse force microscopy (PFM) analysis results exhibit that Aβ fibrils have spiraling piezoelectric domains along the length and a lateral piezoelectric constant of 44.1 pC N-1. Also, the continuous sideband Kelvin probe force microscopy (KPFM) images display that the increment of charge-induced surface potential on a single Aβ fibril is allowed to reach above +1700 mV in response to applied forces.

These findings shed light on the peculiar mechano-electrical surface properties of pathological Aβ fibrils that exceed those of normal body components.*

Both KPFM and nanoindentation measurements were performed using a chemically inert conductive diamond AFM tip. (NanoWorld Pointprobe CDT-FMR).

Vertical and lateral PFM images of Aβ fibrils were obtained by scanning probe microscopy with a platinum/iridium-coated silicon cantilever ( NanoWorld Pointprobe® CONTPt ). The scanning angle of the PFM cantilever was set to zero, with scan rate of 0.5 Hz and loading force of 10 nN. This setup minimized electrostatic contributions to the torsional movement of the tip, allowing measurements to focus on the shear electromechanical effects of Aβ fibrils. Vertical and lateral drive frequencies were 53 kHz and 309 kHz, respectively.*

Figure S10 from „Lateral Piezoelectricity of Alzmeiner‘s Aβ Aggregates by Jinhyeong Jang et al.:
Nanoindentation test result of Aβ fibrils. Direct piezoelectric effects are tested by measuring the surface potential change before and after nano-indentation of Aβ fibrils.
(A) Schematic illustration of the nanoindentation test for Aβ fibrils coated on an Au/Cr substrate.
(B) Topgraphy of Aβ fibrils acquired before and after applying nanoindentation. The post-indentation image shows white spots resulting from physical interactions between the AFM tip and the sample, while the approximate structure of the Aβ fibrils remains intact. Height and potential line sections obtained fom the (c) blue and (d) red lines are shown in the topgraphy of Aβ fibrils. The height remains unchanged, while electrical voltage increment and decrement were observed at the blue and red lines, respectively.
(D) During the nanoindentation the Young‘s modulus of Aβ – fibrils was measured to be 3.17 GPa, closely approxmating the literature (Nanoscale 4, 4426-4429 (2012). Both KPFM and nanoindentation measurements were performed using a chemically inert conductive diamond AFM tip (CDT-FMR, NanoWorld, Switzerland). Collected force curves were analyzed using the Hertz model to estimate the elastic moduli.

*Jinhyeong Jang, Soyun Joo, Jiwon Yeom, Yonghan Jo, Jingshu Zhang, Seungbum Hong and Chan Beum Park
Lateral Piezoelectricity of Alzheimer‘s Aβ Aggregates
Advanced Science, Volume 11, Issue 39, October 024, 2406678
DOI: https://doi.org/10.1002/advs.202406678

Open Access The article “Lateral Piezoelectricity of Alzheimer‘s Aβ Aggregates” byJinhyeong Jang, Soyun Joo, Jiwon Yeom, Yonghan Jo, Jingshu Zhang, Seungbum Hong and Chan Beum Park is licensed under a Creative Commons Attribution 4.0 International License, which permits use, sharing, adaptation, distribution and reproduction in any medium or format, as long as you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons license, and indicate if changes were made. The images or other third party material in this article are included in the article’s Creative Commons license, unless indicated otherwise in a credit line to the material. If material is not included in the article’s Creative Commons license and your intended use is not permitted by statutory regulation or exceeds the permitted use, you will need to obtain permission directly from the copyright holder. To view a copy of this license, visit http://creativecommons.org/licenses/by/4.0/.

Stiffness Mediated-Mechanosensations of Airway Smooth Muscle Cells on Linear Stiffness Gradient Hydrogels

Airflow limitation in obstructive airway disease is characterized by narrowing of the airway lumen from excessive contraction of airway smooth muscle (ASM) and remodeling of the airway wall which includes changes in the extracellular matrix (ECM) of the ASM layer.*

Previous studies on human airway smooth muscle cells ( hASMC ) have independently assessed the influence of extracellular matrix (ECM) proteins on substrates of supra-physiological stiffnesses, such as tissue culture plastic or glass.*

While the influence of discrete substrate stiffness on hASMC behavior has been examined, manipulation of both substrate stiffness and ECM proteins simultaneously (as expected in disease) has not been extensively modeled in vitro.*

In the article “Stiffness Mediated-Mechanosensation of Airway Smooth Muscle Cells on Linear Stiffness Gradient Hydrogels” Yong Hwee Tan, Kimberley C. W. Wang, Ian L. Chin, Rowan W. Sanderson, Jiayue Li, Brendan F. Kennedy, Peter B. Noble and Yu Suk Choi highlight the interplay and complexities between stiffness and ECM protein type on hASMC mechanosensation, relevant to airway remodelling in obstructive airway diseases.*

The authors first determined a physiological range of ASM layer stiffness using a porcine airway and used these empirical recordings to inform the fabrication of a linear stiffness gradient platform coated with different ECM proteins.*

Using this linear stiffness gradient platform, Yong Hwee Tan et al. profiled hASMC morphology, contractile function with alpha-smooth muscle actin (αSMA) and mechanisms of mechanosensation, specifically with nuclear translocalization of Yes-associated protein (YAP) and lamin-A expression.*

Yong Hwee Tan et al.’s assessment of hASMC mechanosensation utilized an innovative hydrogel platform delivering a linear stiffness gradient to understand stiffness-mediated cell behavior with an ECM substrate for cellular adhesion. *

The employment of a stiffness gradient that was designed after empirical measurements performed on ex vivo ASM tissue, enabled the presentation of physiologically relevant stiffnesses to study hASMC behavior.*

Using this platform, the authors of the article found that hASMC mechanosense underlying mechanical cues more than the types of proteins they are anchored to by screening hASMC morphology, contractile phenotype, and mechanomarker expression, with a few exceptions.*

While the authors acknowledge that the findings from their study were done using cells from only one donor they still think that their study provides a proof of concept for the relevance of hASMC mechanosensation to ECM stiffness, and is another step in the right direction for understanding the pathophysiological impact of airway remodeling in obstructive diseases and exploring potential avenues for improving therapy through greater fidelity of in vitro platforms that include key concepts of mechanosensation. *

Yong Hwee Tan et al. wanted to use the same method which is used to assess hydrogel stiffness, namely atomic force microscopy (AFM), to measure ASM stiffness.*

However, nanoscale measurements of ASM strips by AFM proved to be difficult due to an uneven tissue surface after de-epithelialization (Figure S1C, Supporting Information of the cited article), resulting in false force triggering.

To validate the translation of stiffness values measured from macroscale compression (ASM strips) to nanoscale indentation (AFM on hydrogels), Yong Hwee Tan et al. fabricated additional hydrogels of four different stiffnesses using well-characterized polyacrylamide and compared the stiffness of hydrogels measured by uniaxial compression tester and atomic force microscopy (Figure S2A, Supporting Information of the cited article).

The nanoscale stiffness of hydrogels was assessed using an atomic force microscope (AFM) with NanoWorld triangular Pyrex-Nitride PNP-TR AFM probes (the longer AFM cantilever beam – CB 2 – with 200 µm length was used).

These AFM tips probed hydrogels immersed in 1 × PBS with 2 nN, an approach velocity of 2 µm s−1 and a retraction velocity of 10 µm s−1.

Young’s modulus was determined from linear portions of contact-generated force curves using a custom-written code in Igor Pro.

All probe indentations were made in triplicate and averaged for a stiffness measurement in kilopascals (kPa).

An example force curve is shown in Figure S2B, Supporting Information of the cited article. Validation of a linear stiffness gradient was achieved with eight indentations on the hydrogel, 2 mm away from both edges of the hydrogel and at 1 mm intervals along the stiffness gradient axis. Measurements were plotted against displacement from the hydrogel edge (soft to stiff) (Figure 2B of the cited article).

Figure 2 from Yong Hwee Tan et al. 2024 “Stiffness Mediated-Mechanosensation of Airway Smooth Muscle Cells on Linear Stiffness Gradient Hydrogels”:Linear stiffness gradient hydrogel fabrication. A) A schematic of a two-step polymerization process. i) 120 µL of mixed polyacrylamide (PA) solution (% acrylamide + % bis-acrylamide) was added to the primary mold and left to polymerize under ii) a methacrylated coverslip for 20 min. iii) Wedge-shaped 1° gel was removed and flipped for placement of a iv) secondary mold before v) addition of a second 120 µL PA solution and polymerized under a vi) dichlorodimethylsilane-coated coverslip for 20 min. vii) Removal of coverslip and mold completes the fabrication of bi-layered stiffness gradient hydrogel. viii) the dotted arrow indicating the direction of gradient and atomic force microscopy (AFM) measurement. B) Young's moduli gradient measured by AFM. Twelve hydrogels were selected (one gel per batch) and assessed for stiffness, yielding a gradient of 4.0 kPa mm−1, with a range of 1.7 ± 1.2 to 29.6 ± 4.3 kPa (R2 = 0.998, n = 8). Data are presented as mean ± SD. NanoWorld triangular Pyrex-Nitride PNP-TR AFM probes were used to assess the stiffness of the hydrogels with atomic force microscopy.
Figure 2 from Yong Hwee Tan et al. 2024 “Stiffness Mediated-Mechanosensation of Airway Smooth Muscle Cells on Linear Stiffness Gradient Hydrogels”:
Linear stiffness gradient hydrogel fabrication. A) A schematic of a two-step polymerization process. i) 120 µL of mixed polyacrylamide (PA) solution (% acrylamide + % bis-acrylamide) was added to the primary mold and left to polymerize under ii) a methacrylated coverslip for 20 min. iii) Wedge-shaped 1° gel was removed and flipped for placement of a iv) secondary mold before v) addition of a second 120 µL PA solution and polymerized under a vi) dichlorodimethylsilane-coated coverslip for 20 min. vii) Removal of coverslip and mold completes the fabrication of bi-layered stiffness gradient hydrogel. viii) the dotted arrow indicating the direction of gradient and atomic force microscopy (AFM) measurement. B) Young’s moduli gradient measured by AFM. Twelve hydrogels were selected (one gel per batch) and assessed for stiffness, yielding a gradient of 4.0 kPa mm−1, with a range of 1.7 ± 1.2 to 29.6 ± 4.3 kPa (R2 = 0.998, n = 8). Data are presented as mean ± SD.

 

Figure S2 from Yong Hwee Tan et al. 2024 “Stiffness Mediated-Mechanosensation of Airway Smooth Muscle Cells on Linear Stiffness Gradient Hydrogels”:(A) Correlation of Young’s modulus from macroscale stiffness (UCT) assessment with nanoindentation (AFM), was conducted using cylindrical PA hydrogels of different Acrylamide %/Bis-acrylamide % derived from Tse and Engler [47] 10 %/0.06 %, 10 %/0.1 %, 10 %/0.15 % and 10 %/0.3 % (Linear regression, P < 0.0001, R2 = 0.9288, n = 4). Data are presented as mean  SEM. (B) An example force curve from atomic force microscopy with an approach velocity of 2 μm/s, until a 2 nN trigger force was registered, and retraction of indenter at 10 μm/s. NanoWorld triangular Pyrex-Nitride PNP-TR AFM probes were used to assess the stiffness of the hydrogels with atomic force microscopy.
Figure S2 from Yong Hwee Tan et al. 2024 “Stiffness Mediated-Mechanosensation of Airway Smooth Muscle Cells on Linear Stiffness Gradient Hydrogels”:
(A) Correlation of Young’s modulus from macroscale stiffness (UCT) assessment with nanoindentation (AFM), was conducted using cylindrical PA hydrogels of different Acrylamide %/Bis-acrylamide % derived from Tse and Engler [47] 10 %/0.06 %, 10 %/0.1 %, 10 %/0.15 % and 10 %/0.3 % (Linear regression, P < 0.0001, R2 = 0.9288, n = 4). Data are presented as mean  SEM. (B) An example force curve from atomic force microscopy with an approach velocity of 2 μm/s, until a 2 nN trigger force was registered, and retraction of indenter at 10 μm/s.
*Yong Hwee Tan, Kimberley C. W. Wang, Ian L. Chin, Rowan W. Sanderson, Jiayue Li, Brendan F. Kennedy, Peter B. Noble and Yu Suk Choi
Stiffness Mediated-Mechanosensation of Airway Smooth Muscle Cells on Linear Stiffness Gradient Hydrogels
Advanced Healthcare Materials 2024, 2304254
DOI: https://doi.org/10.1002/adhm.202304254

The article “Stiffness Mediated-Mechanosensation of Airway Smooth Muscle Cells on Linear Stiffness Gradient Hydrogels” by Yong Hwee Tan, Kimberley C. W. Wang, Ian L. Chin, Rowan W. Sanderson, Jiayue Li, Brendan F. Kennedy, Peter B. Noble and Yu Suk Choi is licensed under a Creative Commons Attribution 4.0 International License, which permits use, sharing, adaptation, distribution and reproduction in any medium or format, as long as you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons license, and indicate if changes were made. The images or other third-party material in this article are included in the article’s Creative Commons license, unless indicated otherwise in a credit line to the material. If material is not included in the article’s Creative Commons license and your intended use is not permitted by statutory regulation or exceeds the permitted use, you will need to obtain permission directly from the copyright holder. To view a copy of this license, visit https://creativecommons.org/licenses/by/4.0/.