Pointprobe® Silicon-SPM-Probes Available Coatings
|
|
Reflex Coating
|
 |
- 30 nm thick Aluminium coating on the backside
- enhances reflectivity of the laser beam by a factor of 2.5
- prevents light from interfering within the cantilever
- strongly recommended for thin cantilevers if the coating
is compatible with the application
|
|
Hard Magnetic Coating
|
 |
- 40 nm thick Cobalt alloy coating on the tip-side
- permanent magnetization of the tip
- tip needs to be magnetized by means of an external strong magnet
- Soft magnetic samples may be influenced by the tip
|
|
Soft Magnetic Coating
|
 |
- Soft magnetic coating on the tip-side
- coercitivity of app. 0.75 Oe
- remancence magnetization of app. 225 emu/cm3
|
|
Diamond Coating
|
 |
- 100 nm thick coating of polycrystalline diamond on the tip-side
- unsurpassed hardness of the tip
|
|
PtIr5 Coating
|
 |
- 25nm thick double layer of chromium and platinum iridium5
- layer on doth sides of the product
- the layer enhances the conductivity and allows electrical contact
- detector side coating enhances the reflectivity of the laser beam by a factor of 2
- the layer is stress compensated and wear resistant
- bending due to stress is less than 2°
|
|
Gold Coating
|
 |
- 70nm thick chromium/gold coating on the backside of the cantilever
- 70nm thick chromium/gold coating on both sides of the probe
|